材料特性
—
Good uniformity — Fiber distribution is non-directional, enhancing performance evenly | Mechanical properties — Improve the tensile strength, flexural strength and impact toughness of composite materials | Good resin permeability — Easy to resin infiltrate, fast molding speed |
Strong process adaptability — Suitable for various processes such as hand lay-up, compression molding, pultrusion, RTM (resin transfer molding), etc. | Convenient construction — Easy to cut and lay |
Technical Parameters
—
| Item | EMK300/300 | EMK500/300 | EMK500/450 | EMK600/300 | EMK600/450 | EMK800/300 | EMK800/450 |
| Total weight | 609.5 | 809.5 | 959.5 | 909.5 | 960.71 | 1110.71 | 1260.71 |
| Coarse yarn layer | 300 | 500 | 500 | 600 | 600 | 800 | 800 |
Chopped Strand Layer | 300 | 300 | 450 | 300 | 450 | 300 | 450 |
| Sutures | 9.5 | 9.5 | 9.5 | 9.5 | 10.71 | 10.71 | 10.71 |
Application
—