Material properties
—
Alkali resistance — The zirconium glass content is >16.7%, which can resist the corrosion of calcium hydroxide in cement for a long time, ensuring that the fiber will not degrade in an alkaline environment for a long time, and extending the service life of GRC products.  | Crack resistance — Added into cement to form a three-dimensional distributed network structure, effectively inhibiting shrinkage cracking, impact resistance and fatigue resistance, especially suitable for thin-walled or prefabricated parts  | Dispersibility — The chopped fibers do not clump during mixing and are easily mixed with cement mortar to ensure uniform reinforcement and avoid local aggravation or fiber accumulation.  | 
Cement affinity — Surface wetting agent treatment enhances the interface bonding with cement paste and improves the mechanical properties and durability of composite materials  | Easy processing — Can be added dry or wet into concrete, mortar or GRC paste, construction-friendly and adaptable to various processes such as spraying, premixing, and pouring  | 
Technical Parameters
—
| Item | ARC15-170-24MMH | ARC13-2400H | 
| Glass composition | ZrO₂ ≥ 16.5% | ZrO₂ ≥ 16.5% | 
| Line density | 170 tex | 2400 tex | 
| Monofilament diameter | 15 μm | 13 μm | 
| Adaptation process | GRC spraying, premixed, dry-mixed mortar, 3D printing concrete, etc. | Spray molding, pultrusion reinforcement, continuous board making, GRC wet production | 
Application
—